Controllable Morphology and Luminescence Properties of SrMoO4:Sm3+,Na+ Red Emitting Phosphors
Wu Jin-Xiu,Li Mei,Cui Shong-Shong,Liu Zhao-Gang,Hu Yan-Hong,Wang Mi-Tang
DOI: https://doi.org/10.11862/CJIC.2017.036
2017-01-01
Chinese journal of inorganic chemistry
Abstract:With Sm3+ as activator, Na+ as doping charge compensatory, citric acid as complexing agent, ethylene glycol as auxiliary complexing agent by sol-gel method red phosphors precursor was synthesized, then a series of SrMoO4:Sm3+,Na+ red phosphor samples were sintered at 800 degrees C. The crystalline phase, morphology and luminescence properties and quantum efficiency of the samples were characterized by X-ray diffraction, scanning electron microscopy, fluorescence spectrophotometry and fourier transform infrared spectroscopy, respectively. The results show that the synthesized NaSrMoO4:Sm3+ crystallines are a tetragonal structure. The doped ions have little impact on the matrix crystal structure. The emission spectra of the samples are composed of four peaks, 563, 600, 647 and 707 nm belonging to the (5)G(5/2)-> H-6(J)(J=5/2, 7/2, 9/2, 11/2) under the near UV excitation of 403 nm, the relative luminous intensity at 647 nm main emission peak is maximum. When the doping molar fraction of Sm3+ is 1%similar to 3%, the emission intensity is the maximum, luminescence concentration quenching could be observed when the doping molar fraction of Sm3+ ions was more than 1%similar to 3%. The energy transfer type between Sm3+ ions was determined to be the exchange interaction and the critical energy transfer distance (D-c) was calculated to be 1.77 similar to 2.56 nm. In addition, Influences of ethylene glycol on the performance of SrMoO4:Sm3+,Na+ phosphors were investigated in detail. The research result shows that when ethylene glycol addition amount was 5 mL, the sample grains show spherical or elliptical and the structure is uniform and loose and the fluorescence intensity is optimal.