Facet Engineered TiO2 Hollow Sphere for the Visible-Light-mediated Degradation of Antibiotics Via Ligand-to-metal Charge Transfer

Sai Zhang,Zhengliang Yin,Liangxu Xie,Jianjian Yi,Wenjie Tang,Tao Tang,Jinyu Chen,Shunsheng Cao
DOI: https://doi.org/10.1016/j.ceramint.2019.12.142
IF: 5.532
2020-01-01
Ceramics International
Abstract:Efficient removal of tetracycline (TC) under visible-light irradiation over TiO2-based photocatalysts remains a challenge based on the fact that the reported photocatalytic systems still suffer from weak visible-light absorption and/or inefficient charge separation. Herein, we constructed {101} and {001} facets co-exposed TiO2 hollow sphere (001-HT) via a gentle NaF treatment, in which the hollow mesoporous feature can trap incident light for a long time to improve photons efficiently. Meanwhile, the as-formed facet heterojunction significantly facilitates the charge separation. As a result, the 001-HT exhibits a high removal rate (~90.1%) of TC under visible-light irradiation, beyond the values of many reported TiO2-based photocatalysts. Most importantly, we further expound the ligand-to-metal charge transfer mechanism towards TiO2-assisted degradation of TC under visible-light irradiation, which effectively clarifies the confusion about the origin of pure TiO2 visible-light activity towards TC degradation because both TiO2 and TC do not exhibit any visible-light catalytic activity. Therefore, this work provides a new insight in revealing the mechanism of visible-light-mediated TC degradation over pure TiO2 photocatalyst.
What problem does this paper attempt to address?