Effect of stress and temperature on mode of fracture after reheat cracking

V. A. Ferraresi,R. E. Trevisan
1996-12-01
Abstract:The phenomenon of stress-relief cracking or reheat cracking can occur in the heat affected zones (HAZ) or weld fillet during Post Weld Heat Treatment (PWHT). The parts of the HAZ most susceptible to reheat cracking are the coarse-grained regions which result from heating at elevated temperatures in the austenitic region. The aim of the research is to study the effect of stress and temperature during PWHT for stress relief on modes of fractures in High Strength Low Alloy (HSLA) steel produced commercially. The Modified Implant Test was applied along with simulation of thermal cycles typically used for stress-relief treatment of welded components. Basically two different modes of fracture have been identified on basis of fracture appearance. For the temperature range of 500 to 600C, under conditions of high and low stresses, a low-ductility intergranular fracture mode (brittle decohesion) was observed and fracture surfaces were characterized by almost featureless facets. At higher temperatures (680 C) and lower stresses, the fractures were slightly more ductile and occurred by creep cavitation on the grain boundaries. Although intergranular, these fractures were basically dimpled due to coalescence of individual creep cavities. Surfaces of fractures were examined by scanning electron microscopy. Tests with varying initial loadsmore » and different heat-treatment temperatures were realized in order to render separation of stress and temperature effects. It was observed that fracture mode depends mainly on the temperature level rather than on stress range.« less
Engineering,Materials Science
What problem does this paper attempt to address?