Journal of Materials Processing Technology
Abstract:Using basic-type flux cored wires significantly improve the toughness of weld joints, but the addition of fluoride decreases the weld-ability of the metal. In this paper, the flux cored tungsten inert gas (FCTIG) process was used to weld DH36 steel with a basic-type flux cored wire and a rutile-type flux cored wire. The microstructure and mechanical properties of the wires were investigated as well as the diffusible hydrogen content in the different weld joints. The results indicated that the FCTIG process using a basic-type flux cored wire has more technological advantages and produces lower amounts of fume during welding compared with flux cored arc welding (FCAW). The presence of large amounts of alloying elements in the rutile-type flux cored wire promoted the formation of acicular ferrite (AF) in the weld bead, which enhanced the micro-hardness and strength of the bead. The generation of fluoride with the basic-type flux cored wire reduced the diffusible hydrogen content (DHC) in the weld joint, with the lowest DHC value being 3.18 mL/100 g. The toughness of the weld joint made with the basic-type flux cored wire was improved, and the highest impact energy measured was 264.8 J.
What problem does this paper attempt to address?