Spectroscopy and Mode-Locking Laser Operation of Tm:LuYO3 Mixed Sesquioxide Ceramic.
Dongzhen Li,Lingchen Kong,Xiaodong Xu,Peng Liu,Guoqiang Xie,Jian Zhang,Jun Xu
DOI: https://doi.org/10.1364/oe.27.024416
IF: 3.8
2019-01-01
Optics Express
Abstract:Tm:LuYO3 mixed ceramic was successfully fabricated by the solid-state reactive sintering method. The absorption cross section and emission cross section were studied at room temperature. The fluorescence lifetime of F-3(4) energy level was fitted to be 2.6 ms. A continuous-wave (CW) laser operation of Tm:LuYO3 ceramic, pumped at 796 nm, was realized with the output power of 1.2 W and slope efficiency of 25.1%. A mode-locking (ML) laser operation of Tm:LuYO3 ceramic was demonstrated for the first time with pulse duration of 41 ps and pulse repetition frequency of 139.3 MHz. (C) 2019 Optical Society of America under the terms of the OSA Open Access Publishing Agreement