Constructing High-Performance Dielectrics via Molecular and Phase Engineering in Dipolar Polymers
Haoran Xu,Sheng Chen,Shaonan Chen,Rui Qiao,Hui Li,Hang Luo,Dou Zhang
DOI: https://doi.org/10.1021/acsaem.0c02962
IF: 6.4
2021-02-12
ACS Applied Energy Materials
Abstract:When one considers that outstanding dielectric polymers satisfy the developed requirements in the electronic and electrical industries, it is necessary to explore the structure–property relationship of all-organic polymer dielectrics. In this paper, two kinds of side-chain sulfonyl-containing dipolar polymers based on polyolefin main chains, poly{2,5-bis[(4-(methylsulfonyl)phenyl)oxycarbonyl]styrenes} (PBSO<sub>2</sub>) and poly{2,5-bis[(4-(methylsulfonyl)ethyl)oxycarbonyl]styrenes} (PESO<sub>2</sub>), were prepared via radical polymerization. The effect of the side-chain structure on the phase behavior, phase structure, dielectric property, and energy storage of dipolar polymers was investigated. The results showed that PBSO<sub>2</sub> possessed a high glass transition temperature (<i>T</i><sub>g</sub> ≈ 195 °C) and formed the columnar nematic phase owing to the rigid side-chain structure. A dielectric constant of 20.8 (25 °C, 10<sup>3</sup> Hz) was obtained for the polymer PBSO<sub>2</sub> due to the highly orientational polarization and the possible interfacial polarization between the amorphous phase and liquid crystalline phase, which is 18% higher than that of PESO<sub>2</sub>. However, PBSO<sub>2</sub> exhibited a low breakdown strength because of the low band gap of ≈3.46 eV and brittleness of the film. In contrast, a low <i>T</i><sub>g</sub> of 78 °C and isotropic phase were found in the polymer PESO<sub>2</sub>. In addition, a discharge energy density of 6.2 J/m<sup>3</sup> at 270 MV/m was achieved, which was attributed to the high dipole density. This study indicates that it is effective to improve the dielectric constant by introducing a liquid crystalline phase into a dipolar polymer, which offers a route for synthesizing high-performance dielectric polymers.The Supporting Information is available free of charge at <a class="ext-link" href="/doi/10.1021/acsaem.0c02962?goto=supporting-info">https://pubs.acs.org/doi/10.1021/acsaem.0c02962</a>.Testing equipment; SEM images of the cross sections of the polymer films; current density–electric field (<i>J</i>–<i>E</i>) loops; AC conductivity of PBSO<sub>2</sub> and PESO<sub>2</sub> (<a class="ext-link" href="/doi/suppl/10.1021/acsaem.0c02962/suppl_file/ae0c02962_si_001.pdf">PDF</a>)This article has not yet been cited by other publications.
materials science, multidisciplinary,chemistry, physical,energy & fuels