Microstructure, Texture, and Mechanical Properties of Ti-6Al-4V Joints by K-TIG Welding

Shuwan Cui,Yonghua Shi,Tao Zhu,Weicong Liu
DOI: https://doi.org/10.1016/j.jmapro.2018.12.022
IF: 5.684
2019-01-01
Journal of Manufacturing Processes
Abstract:In this study, a Keyhole TIG welding system was successfully used to weld 12 mm thick Ti-6Al-4V alloy workpieces. This technique can be used to weld a single-sided joint using a double-sided forming process, without the preparation of a groove or the use of filler metals. Weld beads with a bright appearance and no obvious defects were formed. The experimental results show that the textures of the α phase in the base metal and weld metal are {0001} <11−20> and {01–10}<2–1–10 > , respectively. Based on the misorientation-angle distribution of the grain boundaries within the α phase, the high-angle grain boundary proportions of the heat-affected zone and weld metal are higher than that of the base metal. The impact toughness of the weld metal is superior to that of the base metal. The high-angle grain boundary proportion has an important influence on the impact toughness of the weld metal. The strength of the weld metal decreased following welding, but it meets the standard of the mechanical properties.
What problem does this paper attempt to address?