Performance of Composite Cathode Sr0.95Ti0.05Co0.95O3-δ-Sm0.2Ce0.8O1.9 Used in Intermediate Temperature SOFCs

YU Lianghao,WANG Xiaoqing,LIN Bin,TIAN Dong,LU Xiaoyong,GU Qingwen,CHEN Yonghong
DOI: https://doi.org/10.14062/j.issn.0454-5648.2015.07.02
2015-01-01
Abstract:A cathode powder of Sr0.95Ti0.05Co0.95O3?δ(STC) and an electrolyte powder of Sm0.2Ce0.8O1.9 (SDC) were synthesized by a citric acid-nitrates self-propagating combustion method. The composite-cathode was obtained by mixing the STC and SDC powders in a mass ratio of 7:3. The chemical compatibility, electrical conductivity and thermal expansion coefficient of the composite cathode were characterized by X-ray diffraction(XRD), direct current four-terminal method and thermal dilatometer, respectively. The XRD results show that a pure cubic STC perovskite phase can be obtained at 900 and℃ no second phase is formed in the composite cathode at the operating temperature. The polarization resistance of the electrode is only 0.05 ?·cm2 at 650 ℃. The anode-supported solid oxide fuel cells of NiO-SDC│SDC│STC?SDC were fabricated. The electrochemical performances were examined at 450?650 ℃ with humidified hydrogen (about 3% H2O) as a fuel and air as an oxidant. It is demonstrated that the anode-supported half cells can be sintered at 1 350 with a dense electrolyte layer and porous℃ electrodes, and the single cell with an open circuit voltage of 0.82 V and the maximum power density of 721 mW/cm2 at 650 ℃ can be obtained. These results indicate that STC?SDC is a promising composite cathode candidate for IT-SOFC with SDC electrolyte.
What problem does this paper attempt to address?