Microstructure, Magnetic and Magnetocaloric Properties of Fe2–x Mn X P0.4Si0.6 Alloys

Yaoxiang Geng,Zhijie Zhang,Ojied Tegus,Chuang Dong,Yuxin Wang
DOI: https://doi.org/10.1007/s40843-016-5125-y
2016-01-01
Science China Materials
Abstract:The present work is devoted to investigating the microstructure, magnetism and magnetocaloric effects of Si- and Mn-rich FeMn(P,Si) alloys. The Mn-substituted alloys with Fe 2– x Mn x P 0.4 Si 0.6 ( x = 1.25, 1.30, 1.35, 1.40, 1.45 and 1.50) were prepared by high-energy ball milling and solid-state reaction. Experimental results show that the alloys crystallized into a majority Fe 2 P-type hexagonal structure, coexisting with minor amounts of (Mn,Fe) 3 Si and (Mn,Fe) 5 Si 3 phases. The Curie temperature decreased linearly from 321 to 266 K with increasingMn content from1.25 to 1.50 in Fe 2– x Mn x P 0.4 Si 0.6 alloys. The first-order magnetic phase transition became weakened and the second-order magnetic phase transition became dominated with increasing Mn content. Fe 0.75 Mn 1.25 P 0.4 Si 0.6 alloy presents a maximum isothermal magnetic-entropy changes of 7.2 J (kg K) –1 in a magnetic field change of 0–1.5 T. The direct measurement shows that Fe0.7Mn1.3P0.4Si0.6 and Fe 0.65 Mn 1.35 P 0.4 Si 0.6 alloys exhibit a maximum adiabatic temperature change of 1.8 K in a magnetic field change of 0–1.48 T. The thermal hysteresis for all alloys is less than 4 K. These experimental results reveal that Fe 2– x Mn x P 0.4 Si 0.6 alloys could be a candidate material for magnetic refrigeration.
What problem does this paper attempt to address?