Colossal and Relaxor-Like Dielectric Behaviors in SrCrO4 Ceramics

J. Sun,S. T. Wang,L. Tong,J. Wang,S. A. Suhaib,Y. M. Xie,G. B. Zhu,C. C. Wang
DOI: https://doi.org/10.1016/j.jallcom.2018.06.094
IF: 6.2
2018-01-01
Journal of Alloys and Compounds
Abstract:Ceramic SrCrO4 samples were prepared via conventional solid state reaction route. Dielectric properties of SrCrO4 were systematically investigated in the frequency range of 10(2)-10(6) Hz and temperature range of 5-900 K. Colossal dielectric behavior near room temperature and relaxor-like dielectric behavior around 730 K with an extremely high dielectric constant up to 1.62 x 10(5) were found. Dual relaxation mechanism composed of a dipolar and a Maxwell-Wagner relaxations is found to be responsible for the colossal dielectric behavior. The dipolar relaxation (R1) is related the defect dipole pair of OHo*-Cr3+ caused by chemically absorbed water. The Maxwell-Wagner relaxation (R2) results from grain boundaries. The relaxor-like dielectric behavior is associated with the hopping motion of oxygen vacancies which leads to a high-temperature relaxation (R3). (C) 2018 Elsevier B.V. All rights reserved.
What problem does this paper attempt to address?