Fatigue Behaviours of the Zirconia Dental Restorations Prepared by Two Manufacturing Methods
Youdong Zhang,Jian-min Han,Gang Zheng,Hong Lin,Wei Bai,Jing Zhao,Zhijian Shen
DOI: https://doi.org/10.1080/17436753.2017.1336365
2017-01-01
Advances in Applied Ceramics
Abstract:The fatigue behaviours were evaluated on a novel zirconia dental restoration known as self-glazed zirconia (SG), prepared by a precision additive 3D gel deposition approach, compared with a conventional zirconia (CZ) restoration, shaped by CNC milling of zirconia blanks made by cold isostatic pressing. Eight fixed partial dentures made by each method were subjected to fracture test, without or with the application of 5-million fatigue cycles, respectively. The processing defects, grain size, and t-m phase transformation were examined by SEM and XRD. The results revealed that the fracture force of the SG restorations was higher than that of the CZ restorations in both cases, which ascribed to the fact that more voids and larger grains in the conventional versus in the SG restorations. The t-m phase transformation was observed only on the fracture surfaces of both materials subjected to fatigue test. Both zirconia restorations meet the clinical requirement.
What problem does this paper attempt to address?