Effect of different refining slag systems on the cleanliness of molten steel for carbon structural steel

S. Zhao,L. Ma,Y. Tao,S.P. He,M.Y. Zhu
DOI: https://doi.org/10.17159/2411-9717/2017/v117n4a5
2017-01-01
Journal of the Southern African Institute of Mining and Metallurgy
Abstract:The effect of two refining slags (A: 1.0-1.8 CaO/Al2O3 ratio, 11-20 wt% SiO2; and B: 1.0-1.2 CaO/SiO2 ratio, 25-35 wt% Al2O3) on the inclusion morphology of a carbon structural steel (Q235B) was studied by controlling the balance between the steel and the refining slag at 1600 degrees C in a Si-Mo resistance laboratory furnace. The results showed that most of the inclusions in the molten steel balanced with slag A were formed by a lowmelting CaO-MgO-Al2O3-SiO2 system with a total oxygen content (T[O]) being fixed at 6-13 ppm. The inclusions in liquid steel balanced with the slag B were mostly formed by the CaO-MnO-Al2O3-SiO2 system, with T[O] controlled to 19-26 ppm. The overall size of the inclusions under balance conditions was higher in the steel reacted with the slag B than that reacted with slag A, with the latter showing more inclusions smaller than 3 m. In order to generate a large number of spherical CaO-MgO-Al2O3-SiO2 inclusions smaller than 3 m while decreasing the T[O] in the resulting steel, the composition of slag A should be used. This composition allowed improving the cleanliness of the slab, and is also advantageous for the castability of the molten steel.
What problem does this paper attempt to address?