Preparation of Highly Textured Bi and MnBi Films by the Pulsed Laser Deposition Method

Zhou Dong,Zhang Yin-Feng,Ma Xiao-Bai,Liu Shun-Quan,Han Jing-Zhi,Zhu Ming-Gang,Wang Chang-Sheng,Yang Jin-Bo
DOI: https://doi.org/10.1088/0256-307x/32/12/127502
2015-01-01
Abstract:Textured Bi and MnBi/Bi thin films are prepared by the pulsed laser deposition method. The highly c-axis textured MnBi films are obtained by annealing the bilayer consisting of textured Bi and Mn films. The coercivities of the MnBi/ Bi film are 1.5T and 2.35T at room temperature and at 373 K, respectively, showing a positive temperature coefficient. Microstructural investigations show that the textured MnBi film results from the orientated growth induced by the textured Bi under-layer.