Study on Ca2+adsorption inhibition of kaolin and quartz in coal slime flotation
DU Ruikang,TUO Biyang,GU Dianfa,WANG Jianli,NIE Guanghua,TANG Yun
DOI: https://doi.org/10.19726/j.cnki.ebcc.202303009
2023-01-01
Abstract:In order to investigate the inhibitory effect of Ca 2+ on other impurity minerals in coal slime and improve the flotation effect, CaCl 2 was used as an inhibitor, while diesel oil and pine oil were employed as collectors and frothers, respectively. Optimal dosages of diesel oil and pine oil are determined to be 1 000 g/t and 300 g/t, respectively. Flotation experiments were conducted on both coal slime and artificially mixed ores to evaluate the inhibitory effect of Ca 2+ on kaolin and quartz in the coal slime. The flotation process followed a single-cell flotation test procedure, and the artificially mixed ore contained 4 g of pure coal mixed with 1 g of kaolin or 1 g of quartz. Prior to commencing the flotation experiment, CaCl 2 solutions with concentrations of 0 mmol/L, 2 mmol/L, 4 mmol/L, 6 mmol/L, 8 mmol/L, 10 mmol/L were added to the slurry. The results show that when the Ca 2+ concentration in coal slime flotation increases from 0 mmol/L to 4 mmol/L, the recovery rate of combustibles increases by 8.24%, signifying a significant inhibitory effect. However, an increase in the Ca 2+ concentration above 4 mmol/L results in an obvious increase in the ash content, which is not conducive to flotation; when flotation is carried out on the mixed ore of pure coal and kaolin, the recovery rate of combustibles increases steadily as the Ca 2+ concentration increases, the recovery rate increases from 87.16% to 96.18%; in terms of the flotation of mixed ore containing pure coal and quartz, the recovery rate of combustibles fluctuates around 91% after the Ca 2+ concentration increases to 4 mmol/L, and the ash content begins to increase significantly; the inhibitory mechanism was analyzed via particle size analysis and Zeta potential testing, the results show that when the Ca 2+ concentration rises from 0 mmol/L to 10 mmol/L, the particle size of kaolin and quartz increases by 0.71 μm and 0.84 μm, respectively, and the absolute value of the Zeta potential of kaolin and quartz decreases by 10.57 mV and 7.98 mV, respectively. The electrostatic repulsion between mineral particles weakens, making them more likely to aggregate; the moderate concentration of Ca 2+ has a better effect on the inhibition of kaolin and quartz, the low concentration of Ca 2+ has no remarkable effect, while high concentration of Ca 2+ will reduce flotation selectivity, increase the ash content of clean coal, and deteriorate the flotation effect.