Influence of Casein Phosphopeptide-Amorphous Calcium Phosphate Application, Smear Layer Removal, and Storage Time on Resin-Dentin Bonding
Jun Lin,Wei-ying Zheng,Peng-ruo-feng Liu,Ning Zhang,Hui-ping Lin,Yi-jing Fan,Xin-hua Gu,Oliver Vollrath,Christian Mehl
DOI: https://doi.org/10.1631/jzus.b1300216
2014-01-01
Abstract:The aim of this study is to evaluate the influence of Tooth Mousse (TM) application, smear layer removal, and storage time on resin-dentin microtensile bond strength (µTBS). Dentin specimens were divided into two groups: (1) smear layer covered; (2) smear layer removed using 15% EDTA for 90 s. In each group, half the specimens were treated once with TM for 60 min. After bonding procedures using a two-step self-etching adhesive (Clearfil SE Bond (CSE); Kuraray Medical, Tokyo, Japan), an all-in-one adhesive (G-Bond (GB); GC Corp, Tokyo, Japan), and a total-etch adhesive (Adper Single Bond 2 (SB); 3M ESPE, St. Paul, MN, USA), the specimens were stored for 3 d or 6 months in deionized water at 37 °C, and µTBS was tested and analyzed. With the exception of SB (no TM application) and GB, the μTBS was significantly increased for CSE and SB using EDTA pre-conditioning and 3 d of storage (P≤0.001). Bond strength of GB decreased significantly when using EDTA (3 d storage, P<0.05). TM application only increased the μTBS of GB (no EDTA) and SB (with EDTA) after 3 d (P≤0.02). Comparing the adhesives after 3 d of storage, CSE exhibited the greatest μTBS values followed by GB and SB (P≤0.02). The factors of adhesive, EDTA, and TM did not show any significant impact on μTBS when specimens were stored for 6 months (P>0.05). The additional application of TM and EDTA for cavity preparation seems only to have a short-term effect, and no influence on µTBS of dentin bonds after a period of 6 months.