Zro2 Nanoparticles Confined in Cmk-3 As Highly Effective Sorbent for Phosphate Adsorption

Xiaoqiu Ju,Jifei Hou,Yuqiong Tang,Yabing Sun,Shourong Zheng,Zhaoyi Xu
DOI: https://doi.org/10.1016/j.micromeso.2016.05.002
IF: 5.876
2016-01-01
Microporous and Mesoporous Materials
Abstract:In the present study, ZrO2 nanoparticles confined in mesoporous carbon CMK-3 (denoted as ZrO2@CMK-3) with varied ZrO2 loading amounts were prepared using the wet impregnation method, and phosphate adsorption on the adsorbents was investigated. For comparison, bulk ZrO2 and activation carbon (AC) supported ZrO2 (denoted as ZrO2/AC) were prepared. The adsorbents were characterized by X-ray diffraction, transmission electron microscopy, N-2 adsorption-desorption, measurement of zeta potential, and X-ray photoelectron spectroscopy. The results showed that loading of ZrO2 into mesoporous carbon CMK-3 led to a remarkable decrease in the pore volume of CMK-3, reflecting effective confinement of ZrO2 in the mesopores of CMK-3. Adsorption kinetics showed that phosphate adsorption on ZrO2@CMK-3 was faster than that on ZrO2/AC. CMK-3 presented very low phosphate adsorption, while ZrO2 and ZrO2-containing adsorbents exhibited very strong phosphate adsorption. Compared with bulk ZrO2, ZrO2/AC and ZrO2@CMK-3 had higher ZrO2 normalized phosphate adsorption capacities. Furthermore, phosphate adsorption was found to be much higher on ZrO2@CMK-3 than on ZrO2/AC. However, nearly identical ZrO2 normalized adsorption amounts were obtained on ZrO2@CMK-3 adsorbents when ZrO2 loading amount increased from 22.74 to 29.49 wt%. As for the reuse of ZrO2@CMK-3, after 4 adsorption desorption cycles ZrO2@CMK-3 exhibited very stable adsorption-desorption performance. (C) 2016 Elsevier Inc. All rights reserved.
What problem does this paper attempt to address?