High‐Energy and Stable Subfreezing Aqueous Zn–MnO 2 Batteries with Selective and Pseudocapacitive Zn‐Ion Insertion in MnO 2

Siyuan Gao,Bomin Li,Haiyan Tan,Fan Xia,Olusola Dahunsi,Wenqian Xu,Yuzi Liu,Rongyue Wang,Yingwen Cheng
DOI: https://doi.org/10.1002/adma.202201510
IF: 29.4
2022-04-28
Advanced Materials
Abstract:One major challenge of aqueous Zn-MnO<sub>2</sub> batteries for practical applications is their unacceptable performance below freezing temperatures. Here the use of simple Zn(ClO<sub>4</sub> )<sub>2</sub> aqueous electrolytes is described for all-weather Zn-MnO<sub>2</sub> batteries even down to -60 °C. The symmetric, bulky ClO<sub>4</sub> <sup>-</sup> anion effectively disrupts hydrogen bonds between water molecules and provides intrinsic ion diffusion even while frozen, and enables ≈260 mAh g<sup>-1</sup> on MnO<sub>2</sub> cathodes at -30 °C . It is identified that subfreezing cycling shifts the reaction mechanism on the MnO<sub>2</sub> cathode from unstable H<sup>+</sup> insertion to predominantly pseudocapacitive Zn<sup>2+</sup> insertion, which converts MnO<sub>2</sub> nanofibers into complicated zincated MnO<sub>x</sub> that are largely disordered and appeared as crumpled paper sheets. The Zn<sup>2+</sup> insertion at -30 °C is faster and much more stable than at 20 °C, and delivers ≈80% capacity retention for 1000 cycles without Mn<sup>2+</sup> additives. In addition, simple Zn(ClO<sub>4</sub> )<sub>2</sub> electrolyte also enables a nearly fully reversible and dendrite-free Zn anode at -30 °C with ≈98% Coulombic efficiency. Zn-MnO<sub>2</sub> prototypes with an experimentally verified unit energy density of 148 Wh kg<sup>-1</sup> at a negative-to-positive ratio of 1.5 and an electrolyte-to-capacity ratio of 2.0 are further demonstrated.
materials science, multidisciplinary,chemistry, physical,physics, applied, condensed matter,nanoscience & nanotechnology
What problem does this paper attempt to address?