Elevated-temperature Tribological Behavior of Ti–B–C–N Coatings Deposited by Reactive Magnetron Sputtering

Xiang-Yang Chen,Shao-Fu Huang,Sheng-Li Ma,Run Huang,Jin Zhang,Hai-Xia Hu
DOI: https://doi.org/10.1007/s12598-015-0640-0
IF: 6.318
2015-01-01
Rare Metals
Abstract:Quaternary Ti–B–C–N coatings with various carbon contents were deposited on high-speed steel (HSS) substrates by reactive magnetron sputtering (RMS) system. The elevated-temperature tribological behavior of Ti–B–C–N coatings was explored using pin-on-disk tribometer, scanning electron microscopy (SEM), and energy-dispersive X-ray spectroscopy (EDX). The present results show that the steady-state friction coefficient value and the instantaneous friction coefficient fluctuation range of Ti–B–C–N coatings decrease as carbon content increases at 100 and 300 °C, while the steady-state friction coefficient value of all Ti–B–C–N coatings becomes higher than 0.4 at 500 °C. As ambient temperature increases, the running-in periods of all Ti–B–C–N coatings become shorter. Wear damage to Ti–B–C–N coatings during sliding at elevated temperature is mainly caused by adhesive wear, and adhesive-wear damage to Ti–B–C–N coatings increases as ambient temperature increases; however, higher carbon content is beneficial for decreasing the adhesive-wear damage to Ti–B–C–N coatings during sliding at elevated temperature.
What problem does this paper attempt to address?