Determination of Optimum Blast Furnace Slag Cooling Rate for Slag Recycling in Cement Manufacture

Y. L. Qin,X. W. Lv,J. Zhang,J. L. Hao,C. G. Bai
DOI: https://doi.org/10.1179/1743281214y.0000000242
IF: 1.7031
2014-01-01
Ironmaking & Steelmaking
Abstract:The crystallisation behaviour of molten blast furnace slag was observed in situ using the single hot thermocouple technique. Isothermal and non-isothermal experiments were conducted to construct the diagrams for time temperature transformation and continuous cooling transformation. The molten slag should be cooled at a minimum critical cooling rate of 10°C s−1. During crystallisation, melilite is the main crystal phase and rankinite is the primary phase. The crystallisation mechanism of the melilite crystal phase involves one-dimensional direction growth with bulk nucleation, whereas the growth mechanism of the rankinite crystal phase is between the surface nucleation mechanism and the one-dimensional direction growth mechanism. The crystallisation activation energies of the melilite and rankinite crystal phases are 238.07±28.81 and 523.52±58.56 kJ mol−1 respectively.
What problem does this paper attempt to address?