Ag/C包覆对Li[Li 0.2 Mn 0.54 Ni 0.13 Co 0.13 ]O 2 电化学性能的影响
薛庆瑞,李建玲,徐国峰,侯朋飞,晏刚,代宇,王新东,高飞
DOI: https://doi.org/10.3866/PKU.WHXB201406251
2014-01-01
Acta Physico-Chimica Sinica
Abstract:A lithium-rich solid-solution layered cathode material, Li[Li0.2Mn0.54Ni0.13Co0.13]O-2, was synthesized using a fast co-precipitation method, and surface modified with Ag/C via chemical deposition. The electrochemical properties, structures, and morphologies of the prepared samples were investigated using X-ray powder diffraction (XRD), field-emission scanning electron microscopy (FESEM), transmission electron microscopy (TEM), galvanostatic charge-discharge cycling, cyclic voltammetry (CV), electrochemical impedance spectra (EIS), and energy dispersive X-ray spectroscopy (EDS). The XRD results showed that the pristine and Ag/C-coated cathode materials both have hexagonal alpha-NaFeO2 layered structures with the R (3) over barm space group. Microscopic morphological observations and EDS elemental mapping showed that a uniform Ag/C coating layer of thickness 25 nm was deposited on the surfaces of Li[Li0.2Mn0.54Ni0.13Co0.13]O-2 particles. The Ag/C-coated Li[Li0.2Mn0.54Ni0.13Co0.13]O-2 material gave an excellent electrochemical performance. The initial discharge capacity (0.05C) of the Ag/C-coated sample was 272.4 mAh.g(-1), with an initial coulombic efficiency of 77.4%, corresponding to 242.6 mAh.g(-1) for the pristine sample, with an initial coulombic efficiency of 67.6%, in the potential range 2.0-4.8 V (vs Li/Li+). After 30 cycles (0.2C), the Ag/C-coated Li[Li0.2Mn0.54Ni0.13Co0.13]O-2 retained a capacity of 222.6 mAh.g(-1), which was 14.45% higher than that of Li[Li0.2Mn0.54Ni0.13CO0.13]O-2. We also found that the Ag/C coating improved the rate capability of the solid-solution material Li[Li0.2Mn0.54Ni0.13Co0.13]O-2. The capacity retention (1C) of the Ag/C-coated sample was 81.3%, compared with the capacity at 0.05C. CV and EIS results showed that the Ag/C coating layer suppressed the oxygen release in the initial charge progress and lowered the surface film resistance and electrochemical reaction resistance of the pristine sample.