Extraction of Metals from A Zinc Smelting Slag Using Two-Step Procedure Combining Acid and Ethylene Diaminetetraacetic Acid Disodium

Kai-qi Jiang,Zhao-hui Guo,Xi-yuan Xiao,Long Zhang
DOI: https://doi.org/10.1007/s11771-012-1212-1
2012-01-01
Abstract:A two-step leaching method in combination of acid and ethylene diaminetetraacetic acid disodium (EDTA-Na 2 ) was applied to extract metals such as Cd, Cu, Fe, Pb and Zn from a zinc smelting slag. The results show that the extraction rates of Cd, Cu, Fe and Zn in slag reach 88.3%, 54.1%, 69.6% and 54.7%, respectively, while the extraction rate of Pb is only 0.05% leached with 1.25 mol/L sulfuric acid under the conditions of the ratio of slag to liquid of 100 g/L, 65 °C and 120 r/min for 2 h. However, Pb extraction rate from 1.25 mol/L sulfuric acid leached residue reaches as high as 66.5% by using 0.1 mol/L EDTA-Na 2 solution. The results indicate that two-step sequential extraction procedure combining 1.25 mol/L sulfuric acid and 0.1 mol/L EDTA-Na 2 solution can extensively extract Cd, Cu, Fe, Pb and Zn from zinc smelting slag.
What problem does this paper attempt to address?