Phase Boundary, Poling Conditions, And Piezoelectric Activity And Their Relationships In (K0.42na0.58)(Nb0.96sb0.04) O-3-(Bi0.5k0.5)(0.90)Zn0.10zro3 Lead-Free Ceramics

Jiagang Wu,Yumei Wang,Hui Wang
IF: 4.036
2014-01-01
RSC Advances
Abstract:Effects of both phase boundaries and poling conditions on the piezoelectric activity of (K,Na)NbO3 (KNN)-based ceramics {e.g., (1 - x) (K0.42Na0.58) (Nb0.96Sb0.04)O-3-x(Bi0.5K0.5)(0.90)Zn0.10ZrO3 [(1 - x) KNNS-xBKZZ]} were studied in detail, and their d(33) was promoted by refining the phase compositions and choosing optimum poling conditions (i. e., poling temperature, poling electric field, and second- poling process). The rhombohedral- tetragonal phase boundary was formed in the ceramics with 0.04 < x <= 0.05. In addition, their piezoelectric activity was further promoted by optimizing the poling temperatures and poling electric fields as well as the second-poling methods. The ceramics with x = 0.045 have enhanced piezoelectric activity (e.g., d(33) similar to 425 pC N-1 and k(p) similar to 47%), and both d(33) (425 pC N-1) and TC (248 degrees C) of this work can match well that (d(33) similar to 416 pC N-1 and T-C similar to 253 degrees C) of textured (Na, K, Li)(Nb, Ta, Sb)O-3 ceramics. It is worth noting that a large strain (0.297%, S-max/E-max = 582 pm V-1) was also found in the ceramics with x = 0.04, which is superior to currently reported results in KNN-based ceramics.
What problem does this paper attempt to address?