Tetragonal-to-Tetragonal Phase Transition in Lead-Free (kxna1−x)nbo3 (x = 0.11 and 0.17) Crystals

Dabin Lin,Zhenrong Li,Fei Li,Changlong Cai,Weiguo Liu,Shujun Zhang
DOI: https://doi.org/10.3390/cryst4020113
IF: 2.7
2014-01-01
Crystals
Abstract:Lead free piezoelectric crystals of (KxNa1−x)NbO3 (x = 0.11 and 0.17) have been grown by the modified Bridgman method. The structure and chemical composition of the obtained crystals were determined by X-ray diffraction (XRD) and electron probe microanalysis (EPMA). The domain structure evolution with increasing temperature for (KxNa1−x)NbO3 (x = 0.11 and 0.17) crystals was observed using polarized light microscopy (PLM), where distinguished changes of the domain structures were found to occur at 400 °C and 412 °C respectively, corresponding to the tetragonal to tetragonal phase transition temperatures. Dielectric measurements performed on (K0.11Na0.89)NbO3 crystals exhibited tetragonal to tetragonal and tetragonal to cubic phase transitions temperatures at 405 °C and 496 °C, respectively.
What problem does this paper attempt to address?