Microstructure and mechanical properties of (TiB+La2O3)/Ti composites heat treated at different temperatures

GUO Xiang-long,WANG Li-qiang,QIN Ji-ning,Lü Wei-jie,ZHANG Di
DOI: https://doi.org/10.1016/S1003-6326(14)63247-7
IF: 3.752
2014-01-01
Transactions of Nonferrous Metals Society of China
Abstract:Near-αtitanium matrix composites reinforced with TiB and La2O3 were synthesized by common casting and hot-working technology. The effects of β heat treatment temperature on the microstructure and the tensile properties of the in situ synthesized (TiB+La2O3)/Ti were studied. Microstructure was studied by OM and TEM, and tensile tests were carried out at room temperature and 923 K, respectively. Results show that with the increase ofβheat treatment temperature, priorβphase grain size increases andαcolony size decreases. Room temperature tensile strength increases with the increase ofβheat treatment temperature, which can be attributed to the decrease of α colony size with the increase of β heat treatment temperature. However, high-temperature tensile strength decreases with the increase ofβheat treatment temperature and the decrease of the high-temperature tensile strength is due to the increase of the priorβphase grain size.
What problem does this paper attempt to address?