On The Characteristic Length Scales Associated With Plastic Deformation In Metallic Glasses

p murali,y w zhang,h j gao
DOI: https://doi.org/10.1063/1.4717744
IF: 4
2012-01-01
Applied Physics Letters
Abstract:Atomistic simulations revealed that the spatial correlations of plastic displacements in three metallic glasses, FeP, MgAl, and CuZr, follow an exponential law with a characteristic length scale l(c) that governs Poisson's ratio nu, shear band thickness t(SB), and fracture mode in these materials. Among the three glasses, FeP exhibits smallest l(c), thinnest t(SB), lowest nu, and brittle fracture; CuZr exhibits largest l(c), thickest t(SB), highest nu, and ductile fracture, while properties of MgAl lie in between those of FeP and CuZr. These findings corroborate well with existing experimental observations and suggest l(c) as a fundamental measure of the shear transformation zone size in metallic glasses. (C) 2012 American Institute of Physics. [http://dx.doi.org/10.1063/1.4717744]
What problem does this paper attempt to address?