Abstract:We report the synthesis and single-crystal X-ray diffraction, magnetic, and luminescence measurements of a novel family of luminescent cage-like tetranuclear silsesquioxanes (PhSiO 1.5 ) 8 (LnO 1.5 ) 4 (O)(C 5 H 8 O 2 ) 6 (EtOH) 2 (CH 3 CN) 2 ⋅2CH 3 CN (where Ln = Tb, 1 ; Tb/Eu, 2 ; and Gd, 3 ), featuring seven-coordinated lanthanide ions arranged in a one-capped trigonal prism geometry. Compounds 1 and 2 exhibit characteristic Tb 3+ and Tb 3+ /Eu 3+ -related emissions, respectively, sensitized by the chelating antenna acetylacetonate (acac) ligands upon excitation in the UV and visible spectral regions. Compound 3 is used to assess the energies of the triplet states of the acac ligand. For compound 1 , theoretical calculations on the intramolecular energy transfer and multiphonon rates indicate a thermal balance between the 5 D 4 Stark components, while the mixed Tb 3+ /Eu 3+ analog 2 , with a Tb:Eu ratio of 3:1, showcases intra-cluster Tb 3+ -to-Eu 3+ energy transfer, calculated theoretically as a function of temperature. By utilizing the intensity ratio between the 5 D 4 → 7 F 5 (Tb 3+ ) and 5 D 0 → 7 F 2 (Eu 3+ ) transitions in the range 11–373 K, we demonstrate the realization of a ratiometric luminescent thermometer with compound 2 , operating in the range 11–373 K with a maximum relative sensitivity of 2.0% K −1 at 373 K. These findings highlight the potential of cage-like silsesquioxanes as versatile materials for optical sensing-enabled applications.
chemistry, multidisciplinary