An improved deresining method for semithin sections embedded-epoxy resin

Hai-ying JIANG,Ming SHEN,De-yun FENG
DOI: https://doi.org/10.3321/j.issn:1672-7347.2000.01.029
2000-01-01
Abstract:Deresining must be performed for HE, specific histochemical staining and immunohistochemical detection on semithin-sections embedded-epoxy resin. The deresining process in general methods had to take 24 hours, and the semithin-sections were easily separated from slides. An improved method was introduced in this paper, by which deresining time was only 5 minutes, and it could also avoid the separation of semithin-sections from the slides. The staining result was very good, and the resolving power of images was high.
What problem does this paper attempt to address?