Enhancing Internal Electric Field of 3D Porous Chitosan-Pdi Polymer with Donor-Acceptor Structure for Efficient Photocatalytic Advanced Oxidation
Sijie Huang,Hanjie Zhang,Wenting Li,Liping Liu,Jingyi Xu,Meichi Chong,Junshan Li,Yongfa Zhu
DOI: https://doi.org/10.1016/j.apcatb.2024.123790
2024-01-01
Abstract:The charge separation efficiency of photocatalysts remains a formidable challenge for visible light-driven advanced oxidation. Herein, a three-dimensional (3D) porous PDI-CTS photocatalyst with donor-acceptor (D-A) structure was synthesized and showed an impressive bisphenol A (BPA) degradation rate of 0.343 min(-1) through peroxydisulfate (PDS) activation. The D-A interaction facilitates charge transfer from CTS to PDI, inducing a larger molecular dipole moment than pure PDCTA. Thus, robust internal electric field with 6.9 times enhancement was built up in PDI-CTS, facilitating the separation of photogenerated carriers. Moreover, multiple PDI active sites provided by 3D porous PDI-CTS were conducive to the adsorption of pollutants, and generated more electron-enriched PDI(-) for PDS activation. Since PDS captures electrons from PDI(-), the migration of holes to the surface is further improved, resulting in a remarkable mineralization rate of 87%. This work develops a unique D-A photocatalyst to promote photogenerated carriers migration for efficient photocatalytic advanced oxidation.