Abstract:Charging overpotential, which is still relatively too high for non-aqueous electrolyte lithium-air batteries, can be extremely low at high test temperatures. The charging overpotential decreases with the increase of test temperature from 303 K to 343 K. Charging voltage plateau is about 3.1 V and 3.6 V under the current density of 100 mA g-1 and 500 mA g-1, respectively, at the test temperature of 343 K. X-ray diffraction is carried out to prove the oxidative decompositions of Li2O2 during the charging process. The results of electrochemical impedance spectroscopy indicate the influence of test temperature on the charge-transfer resistance. This discovery could lead to new development orientation of lithium-air battery.