Microwave-assisted synthesis and photocatalytic activity of quantum-sized ZnO

Wenguo Xu,ChengXiang Ma,Shixiang Lu,Lian Dai,Haifeng Zhang
DOI: https://doi.org/10.4028/www.scientific.net/AMR.284-286.866
2011-01-01
Abstract:ZnO was prepared using zinc acetate dehydrate (Zn(CH3COO)(2)center dot 2H(2)O) and lithium hydroxide monohydrate (LiOH center dot H2O) as raw material through a microwave-assisted sol-gel method. The prepared ZnO presents the wurtzite structure. The influence of different reaction temperature and heating time to the size of ZnO was researched. The photocatalytic activity of ZnO was evaluated by the degradation rate of C.I. Reactive Blue 4 in aqueous solution. The particle size of ZnO is about 4.33 nm at the reaction condition of 50 degrees C for 10 min and the photoeatalytic performance is the best. The degradation rate of C.I. Reactive Blue 4 could exceed 75% in 30 min at room temperature when the initial concentration of C.I. Reactive Blue 4 was 40 mg/L and the concentration of the quantum-sized ZnO was 0.1 g/L.
What problem does this paper attempt to address?