Abstract:Three incongruent melting La(w)Nd(x)Gd(y)Y(z)Sc(4-w-x-y-z)(BO(3))(4) (LGYSB:Nd) crystals with different Y concentrations (z = 0.15, 0.05, and 0.025) have been grown by the Czochralski method for the first time. The LGYSB:Nd-type crystals exhibit an acentric structure similar to that of the natural mineral huntite CaMg(3)(CO(3))(4), with space group R32. The composition of the LGYSB:Nd_3 (z = 0.025) crystal grown from the starting melt composition...