Bio-oxidation of arsenic and stibium bearing gold ores

Qian Li,T. Jiang,Gaunzhou Qiu,YongBin Yan,G. H. Li
2010-01-01
Abstract:Bio-oxidation of arsenic and stibium bearing gold ores with acidithiobacillus ferrooxidans was studied. The preoxidation results show that the best bio-oxidation technical parameters are the initial pH in the range of 1.8 ~ 2.0, particle sizes under 0.074 mm, temperature in the range of 25 °C ~ 30°C and rotating speed of the orbital incubator in 100 rpm ~ 160 rpm. The leaching results show that If the ore, of which contain 10.37 per cent arsenic and 36.81 per cent stibium, is not bio-oxidised, gold leaching is only about 41 per cent, after 8 days oxidised, the result is about 76.55 per cent, which improved about 35.62 points. The relationship between gold leaching and arsenic oxidation is direct proportion, furthermore, it needs only partly oxidise and higher gold leaching could be get, for example, gold leaching is over 90 per cent when asenic oxidation is 60 per cent. The results will provide theoretical and technological supports of bio-oxidation arsenopyrite for pretreating refractory gold ores.
What problem does this paper attempt to address?