Microscopic phase field simulation for the evolution of antisite defect of Ll2 structure and DO22structure in Ni75Al5.3V19.7 alloy

Jing Zhang,Zheng Chen,Yongxin Wang,Yanli Lu,Jinliang Liang Huo,Huihui Zhen,Yan Zhao
2009-01-01
Abstract:The antisite defect for L12-structure Ni3 Al and DO22-structure Ni3V of Ni7.5Al5.3V19.7 alloy is studied by microscopic phase field method in this paper. The results show that the concentration of antisite defects AlNi, VNi and NiAl for L12 structure, VNi, AlNi, NiV and AlV for DO22 structure all decrease with precipitate process and reach to equilibrium values at the early stage of precipitation respectively. With the elapse of time, the two structures grow up while the concentrations of antisite defects always keep unchanged. The concentrations of equilibrium state antisite defects AlNi and VNi for L12 structure α site, VNi and AlNi for DO22 structure α site are of the 10-2 order, and antisite defect Nial for L12 structure β site, NiV for DO22 structure β site are of 10-1 order, the two defects being the main antisite defects for the L12 and DO22 structures. The addition element has a great site-preference for a certain ordered phase, V atom prefers to occupy L12 structure β site while Al atom prefers to occupy DO22 structure α site. © 2009 Chin. Phys. Soc.
What problem does this paper attempt to address?