An Approach to Control the Interlamellar Bonding of Plasma-Sprayed Y2O3-ZrO2 Coatings Through Deposition Temperature

C.-J. Li,Y.-Z. Xing,C.-X. Li,G.- J. Yang
DOI: https://doi.org/10.31399/asm.cp.itsc2009p0957
2009-01-01
Abstract:Abstract Plasma-sprayed ceramic coatings exhibit a lamellar structure with a mean bonding ratio of less than 32%, which dominates coating properties and limits the performance that can be achieved. In this study, yttria-stabilized zirconia (YSZ) coatings were plasma sprayed at different deposition (substrate surface) temperatures up to a maximum of 1100 °C. The lamellar mean bonding ratio, estimated from the ionic conductivity of the YSZ coatings, was found to increase from 32% in room temperature deposits to more than 75% in the deposits prepared at 1100 °C. Evidence of this improvement is also observed in fractured deposit cross-sections. The results show that controlling deposition temperature is an effective way to optimize lamellar interface bonding and, as a result, coating properties.
What problem does this paper attempt to address?