Recovery of Fine Scheelites from Flotation Tailings by Flotation Column

黄光耀,冯其明,欧乐明,卢毅屏,张国范
DOI: https://doi.org/10.3969/j.issn.0258-7076.2009.02.025
2009-01-01
Abstract:In order to recover fine scheelites from flotation tailings of cleaner circuit, a novel flotation column, which using microcellular material as bubble generator and using expert system to control key work parameters of the column, was manufactured.Pilot and full scale column flotation experiments were carried out, and interrelated work parameters of the column were obtained.The optimum work parameters are as follows:the superficial velocity of the feed 0.27 cm/s and the superficial velocity of air 1.57 cm/s.The recovery of WO3 reaches 43.41% with an average grade of 24.52%, and the enrichment ratio reaches 35.03.The recoveries of three different size fraction, 5-10 μm, 10-19 μm and 19-38 μm, all reach 65%.Sauter diameter of the bubbles in the column is about 400 μm, and smaller diameter make the flotation rate constant k increases greatly, improving flotation performance, which is the key reason that fine scheelites can be recovered.
What problem does this paper attempt to address?