Novel iron heparin anticoagulation coating for intravascular stents

Meng Liu,Lei Xing,Zhi-fei Dai,Yan Ma,Shao-qin Liu,Yu Li
DOI: https://doi.org/10.3321/j.issn:1673-8225.2008.48.020
2008-01-01
Abstract:The experiment was performed at Nanomedicine and Biosensor Laboratory of Harbin Institute of Technology from December 2006 to January 2008. Fe3+/heparin multilayer films were assembled on the surface of Ni-Ti alloy by the layer-by-layer self-assembly, which made the stable glucose-Fe complex coating form on the surface of Ni-Ti alloy. The ultraviolet-visible absorption spectrophotometry, atomic force microscopy and fourier transform infrared spectroscopy proved that the Fe3+/heparin could form uniform multilayer films by alternative deposition on the surface of Ni-Ti alloy, and the coating had good stability. Studies showed that the increase of pH value and ionic strength in solution could obviously improve the increasing speed of the coating. The coating had good anticoagulation property and blood compatibility, which were proved by detection of thrombin inactivation, activated partial thromboplastin time, hemolysis test and platelet adhesion test. The heparin did not decrease its anticoagulation property after combined with Fe3+. The results suggested that the coating could be use for the surface modification of intravascular stents, and prevent thrombosis forming in early stage of stent implantation.
What problem does this paper attempt to address?