Structure and Properties of Oxidized Flax Fiber Treated with Sericin Solution
Yan Zhang,Hong Lin,Yuyue Chen
DOI: https://doi.org/10.3993/tbis2008020
2008-01-01
Abstract:In order to achieve the protein property of flax fiber, the flax fiber was selectively oxidized with NalO(4), and then the oxidized flax fiber was treated with sericin solution. Different factors, such as concentration of sericin solution, pH value, treating time and treating temperature affecting on weight gain, the breaking strength and the breaking elongation of flax fiber were discussed. The structure of sericin proteinic flax fiber was investigated by SEM, FT-IR and XRD analysis. The results indicated that the weight gain of the oxidized flax fiber increased during sericin treatment, but little change was found on the breaking strength and the breaking elongation of the oxidized flax fiber treated with sericin solution. FR-IR spectra indicated that a characteristic absorption band of the aldehyde group was formed after oxidizing the flax fiber and the Schiff's base was formed between the aldehyde group and amino group in the sericin main chain after treating with sericin solution. XRD analysis showed that the crystallinity of the flax fiber changed slightly after treating with sericin solution.
What problem does this paper attempt to address?