Influences of Special Components on Solidification Temperature and Crystallizing Properties of Low Fluorine Mould Fluxes

WANG Qian,XIE Dan,HE Sheng-ping,WANG Ping
DOI: https://doi.org/10.3321/j.issn:1001-0963.2007.06.009
2007-01-01
Abstract:The mould fluxes with high fluoride content not only aggravate the etch of submerged entry nozzle, but also bring about environmental hazards. None fluorine and Low fluorine mould fluxes should be developed. In order to avoid the property deterioration of mould fluxes without fluoride, substitutions for fluoride should be harmonized with the casting function of mould fluxes. Comparing with high fluoride mould fluxes, four series of low fluorine mould fluxes were developed. By testing the melting point, viscosity, breaking temperature, crystallizing temperature and crystallizing proportion, and analyzing experimental data, the results were as follows: B 2O 3, Li 2O, Cr 2O 3 and TiO 2 can be used to partly replace CaF 2 to get mould fluxes containing 4.5% of CaF 2; CeO 2 cannot replace CaF 2.
What problem does this paper attempt to address?