Physical Properties of Diamond Coatings on A Wc-6%Co Substrate
S Liu,DQ Yi,ZM Yu
DOI: https://doi.org/10.1088/0256-307x/19/3/341
2002-01-01
Chinese Physics Letters
Abstract:We have investigated the physical properties, including the morphology, texture, adhesion and chemical quality, of high-frequency chemical vapour deposited diamond coatings on WC-6%Co substrates, which were pre-treated by a two-step etching method. The results indicate that the increasing Co content from 0.12 to 3.05% within the etching depth of 5 mum caused a morphology transformation from prism diamond to spherulitic diamond, and a texture transformation from a {111} orientation to a (110) orientation. The Raman spectrum shows that the spherulitic diamond film contains more non-diamond phases (graphite, amorphous carbon and diamond-like carbon, etc) and has lower chemical quality than diamond films on a WC-6%Co substrate. The diamond coating grain sizes became about four times smaller when the deposition temperatures on the substrate surface were reduced from 1000 to 900degreesC. Compared with spherulitic diamond films, the prism diamond films exhibit better adhesion on the WC-6%Co substrate.
What problem does this paper attempt to address?