Magnetic Properties and Magnetocaloric Effect of Nd<sub>0.7</sub>Gd<sub>0.3</sub>Mn<sub>2</sub>Si<sub>2</sub> Alloy
Shi Dong Lin,Xiao Long Chen,Jiang Wang,Chao Zhu,Maohua Rong,G. H. Rao,Haijun Zhou
DOI: https://doi.org/10.4028/www.scientific.net/amr.1142.47
2017-01-01
Advanced Materials Research
Abstract:In this work, crystal structure, magnetic properties and magnetocaloric effect of Nd 0.7 Gd 0.3 Mn 2 Si 2 alloy were studied by X-ray diffraction (XRD), Physical Property Measurement System (PPMS) and Differential Scanning Calorimetry (DSC). Nd 0.7 Gd 0.3 Mn 2 Si 2 crystallizes in ThCr 2 Si 2 -typed structure with space group I4/mmm, in which the Nd, Gd, Mn and Si atoms occupy 2a (0, 0, 0), 2a (0, 0, 0), 4d (0, 1/2, 1/4) and 4e (0, 0, 0.38261) position, respectively. The Curie temperature (Tc) of Nd 0.7 Gd 0.3 Mn 2 Si 2 alloy is 42 K, while the spin reorientation temperature (T SR ) is 26 K and the Nel temperature (T N ) is 410 K. The Tc and T N were determined using PPMS and DSC, respectively. The maximum value of the magnetic entropy change (-S m ax ) in the field change of 0-5 T is 11.862 J/kg K, while the value of relative cooling power (RCP) in Nd 0.7 Gd 0.3 Mn 2 Si 2 alloy is 69.666 J/kg under the field change of 5 T.