Cavitation-erosion Resistance of Arc Ion-plated Hard Coatin gs

PAN Guo-shun,YANG Wen-yan,SHAO Tian-min,WANG Yi-min
DOI: https://doi.org/10.3321/j.issn:1004-0595.2001.01.004
2001-01-01
Abstract:The cavitation-erosion behavior of TiN, CrN and (Ti,Cr)N hard coatings produced by arc ion-plating on the surface of grey cast iron was studied with an ultrasonic cavitation-erosion testing apparatus and a scanning electron microscope. The results indicate that the surface roughness of the substrate, the surface morphology of the coating, substrate bias voltage, a nd the thickness of the coating have different influence on the cavitation-eros ion behavior of the coatings. Shielded ion plated (Ti,Cr)N multi-component coat ing shows better cavitation-erosion resistance than TiN and CrN coatings becaus e of their higher microhardness and decreased amounts of micro-defects. (Ti,Cr) N coating of about 3 μm thick deposited at Vs=300 V shows better resistan ce to cavitation-erosion as compared with the same coating of different thickn ess.
What problem does this paper attempt to address?