Mechanical Relaxation in Srbi2ta2o9 Ceramics

F Yan,YI Wang,JS Liu,ZG Zhang,XB Chen
DOI: https://doi.org/10.1063/1.124016
IF: 4
1999-01-01
Applied Physics Letters
Abstract:The internal friction (IF) of SrBi2Ta2O9 ceramics was measured by using the reed vibration method in the temperature range from 100 to 600 K with frequency in kilohertz. A high IF peak appeared around 500 K, which was interpreted in terms of the migration of oxygen vacancies. Another low IF peak was found with a peak temperature of 200–250 K, which varied for tens of degrees in different samples. This peak was assumed to be due to the depinning process of domain walls from oxygen vacancies. These results are helpful in the understanding of the excellent fatigue resistance property of SBT at room temperature.