Magnetoresistive Polyaniline/multi-Walled Carbon Nanotube Nanocomposites with Negative Permittivity.

Hongbo Gu,Jiang Guo,Qingliang He,Yuan Jiang,Yudong Huang,Neel Haldolaarachige,Zhiping Luo,David P. Young,Suying Wei,Zhanhu Guo
DOI: https://doi.org/10.1039/c3nr04152b
IF: 6.7
2014-01-01
Nanoscale
Abstract:Contrary to the observed positive giant magnetoresistance (GMR) in as-received multi-walled carbon nanotubes (MWNTs), pure polyaniline (PANI) synthesized with Cr(vi) as oxidant and MWNTs/PANI nanocomposites with ammonium persulfate (APS) as oxidant, a room temperature negative GMR of around -2% was reported in MWNTs/PANI nanocomposites with Cr(vi) as oxidant. Different from a frequency switch of permittivity from negative to positive in MWNTs/PANI nanocomposites with APS as oxidant, unique negative permittivity was observed in MWNTs/PANI nanocomposites with Cr(vi) as oxidant within the measured frequency range from 20 to 2 × 10(6) Hz. The obtained unique negative permittivity was explained by the plasma frequency from the Drude model, at which the permittivity changes from negative to positive and the material changes from a metamaterial to an ordinary dielectric medium. The observed positive and negative GMR behaviors in these disordered systems as verified by the temperature dependent resistivity exploration were well explained through a wave-function shrinkage model and orbital magnetoconductivity theory by calculating the changed localization length (a0).
What problem does this paper attempt to address?