Metal Cation-Promoted Hydrogen Generation in Activated Aluminium Borohydride Ammoniates

Ziwei Tang,Yingbin Tan,Hui Wu,Qinfen Gu,Wei Zhou,Craig M. Jensen,Xuebin Yu
DOI: https://doi.org/10.1016/j.actamat.2013.05.003
IF: 9.4
2013-01-01
Acta Materialia
Abstract:The crystal structure of an aluminum-based borohydride ammoniate - Al(BH4)(3)center dot 6NH(3) - is reported for the first time. The molecular structure of Al(BH4)(3)center dot 6NH(3) is resolved by high-resolution X-ray diffraction. The compound crystallized in the space group Pbcn (No. 60), with lattice parameters of a = 13.2824(5) angstrom, b = 15.2698(7) angstrom and c = 13.1848(6) angstrom. Structure analysis shows that this compound contains complex hexamminealuminum (III) [Al(NH3)(6)](3+) cations, which are surrounded by BH4- anions. The interatomic distances between the H delta+ s from the NH3 units and the H delta- s from the BH4 units are in the range of 1.91-2.19 angstrom, suggesting the presence of significant H delta+ ... H-delta interactions. Mass spectrometry, thermogravimetry and temperature-programmed desorption studies of metal cation-modified aluminum-based borohydride ammoniates using the reactions of various metal borohydrides M(BH4)(n) (M = Na, Li, Ca, Mg) and chlorides MCln (M = Sc, Ni, Cu, Zn, Mg, Ca, Li) reveal that their dehydrogenation properties are strongly dependent on the polarizing power of the added metal cations. It is hypothesized that the added metal cations may activate the borohydride ion to such an extent that its H delta- can easily react with the H delta+ of the [Al(NH3)(6)](3+) cation, resulting in an enhanced interaction between the H delta+ and H delta-, thus enhancing their dehydrogenation kinetics. Subsequent deuterium isotope and X-ray measurements support the hypothesis that the H delta+ ... H-delta interactions play a role in the dehydrogenation of the metal borohydride ammoniates. Of the systems investigated, 0.5Mg(BH4)(2)/Li2Al(BH4)(5)center dot 6NH(3) is notable as it releases more than 10 wt.% high-purity H-2 within 30 min below 120 degrees C. This ranks among the highest values currently reported for potential solid-state hydrogen storage materials. These findings provide a feasible and simple route for modifying B-N-based, lightweight materials for highly efficient dehydrogenation. (C) 2013 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.
What problem does this paper attempt to address?