Deformation behavior of Al-6.1Zn-2.8Mg-1.9Cu-0.25Cr alloy during hot compression

XIA Qing-kun,LIU Zhi-yi,LIN Liang-hua,YuShu Liu,XU Xiao-chang,Xu Chen
2013-01-01
Abstract:The flow stress behavior of Al-6.1Zn-2.8Mg-1.9Cu-0.25Cr alloy was studied by the isothermal compression of cylindrical specimen at 300-500°C and strain rate range of 0.01-1 s-1 on a Gleeble-1500 simulated machine. The thermal deformation constitutive equations were established, and the microstructure of the alloy was characterized by TEM. The results show that the flow stress decreases with the increasing of deformation temperature and increases with increasing strain rate. When the temperature range is 360-400°C, dynamic recovery is dominant during hot compression. However, when the deformation temperature is over 400°C, dynamic re-crystallization occurrs. When the strain rate is 0.01-1 s-1, no effect on deformation softening mechanism of the alloy is observed, but obvious effect of strain rate on the substructure of the alloy is examined. With the increasing of the strain rate the dislocation density increases, while the sub-grain size decreases. The recommended deformation temperature and strain rate for Al-6.1Zn-2.8Mg-1.9Cu-0.25Cr alloy are 380-400°C and 0.1 s-1.
What problem does this paper attempt to address?