Preparation of Acicular Wollastonite Using Hydrothermal and Calcining Methods

H. Wu,J. Yang,H. W. Ma,M. W. Wang
DOI: https://doi.org/10.1080/10584587.2013.789777
2013-01-01
Integrated Ferroelectrics
Abstract:The acicular wollastonite was prepared successfully using the NaSiO39H2O and Ca(OH)2 as raw materials via two-step hydrothermal synthesis and calcination methods. The scawtite and xonotlite were synthesized by two-step hydrothermal processes successively. The acicular wollastonite was prepared by the synthesized xonotlite after calcination. The hydrothermal-treated temperature, the water-solid ratio and the reaction time were studied for obtaining the xonotlite. The wollastonite powder was characterized by XRD, SEM and Differential Thermal Analysis. The results showed that the acicular wollastonite powder could be prepared efficiently after the hydrothermal treatment of 260 degrees C for 2hours with 6:1 water-solid ratio using the synthesized scawtite and calcination of the synthesized xonotlite by 800 degrees C for 2hours.
What problem does this paper attempt to address?