Magnetoelectric Coupling of Terfenol-D/P(Vdf-Trfe)/Terfenol-D Laminates Mediated by Crystallite Size of Electroactive Polymer

F. Fang,S. C. Shan,W. Yang
DOI: https://doi.org/10.1007/s00707-013-0860-z
IF: 2.645
2013-01-01
Acta Mechanica
Abstract:The attention here is focused on the magnetoelectric (ME) coupling in Terfenol-D/P(VDF-TrFE)/Terfenol-D laminated composites. The electroactive P(VDF-TrFE) 75/25mol% copolymer films were prepared using three different annealing conditions: 135°C for 2h , 6h and 140°C for 2h. The results show that the laminate with the copolymer film annealed at 135°C for 2h exhibits the highest ME coupling, while the one with the copolymer film annealed at 140°C for 2h shows the lowest. Microstructure examination demonstrates that the crystallites grow significantly in size with either the annealing time or the temperature although the crystallinity increases slightly. It is suggested that the copolymer film with smaller crystallite size, or higher volume fraction of the amorphous/crystallite interfacial layers, is beneficial to the piezoelectric effect and consequently the ME coupling of the laminated composites.
What problem does this paper attempt to address?