Growth and electrical properties of 0.95Na 0.5Bi 0.5TiO 30.05K 0.5Bi 0.5TiO 3 lead-free piezoelectric crystal by the TSSG method

Di Lin
DOI: https://doi.org/10.1016/j.jcrysgro.2011.12.073
IF: 1.8
2012-01-01
Journal of Crystal Growth
Abstract:0.95Na0.5Bi0.5TiO3–0.05K0.5Bi0.5TiO3 lead-free piezoelectric single crystal with rhombohedral structure was grown by the top-seeded solution growth method. The temperature dependence of dielectric constant and loss, polarization hysteresis loops, the optimum poling condition and the electromechanical coupling property were investigated for the 〈100〉-oriented as-grown crystal. The curves ε(T) show two anomalies, which are related to the two phase transformations at the temperature range of 130–340°C. The piezoelectric constant d33 and electromechanical coupling coefficient kt for the 〈001〉-oriented crystal at room temperature reached 147pC/N and 0.52, respectively. The value of kt demonstrated a relatively stable thermal electromechanical coupling property over the temperature range of 15–130°C.
What problem does this paper attempt to address?