Effects of Heat Treatments on the Microstructure and Mechanical Properties of As-Extruded Tibw/Ti6al4v Composites

B. Wang,L. J. Huang,L. Geng
DOI: https://doi.org/10.1016/j.msea.2012.08.071
2012-01-01
Abstract:In order to further exploit the superior mechanical properties of in situ formed TiBw/Ti6Al4V composites, solution and aging heat treatments were performed on the as-extruded composites. The results show that, with increasing solution treatment temperatures, the volume fraction of primary α phase decreases, while that of the transformed β phase increases correspondingly. Both the size and volume fraction of the fine α and β phases formed from the quenched martensite phase increased with increasing aging temperatures. The hardness and tensile strength of the composites increased on increasing the solution temperature from 930 to 990°C; however, both decreased on increasing aging temperature from 500 to 700°C. A superior combination of tensile strength (1365MPa) and elongation (7.9%) of the as-extruded 5vol% TiBw/Ti64 composite has been obtained by water quenching from 990°C and aging at 600°C for 6h.
What problem does this paper attempt to address?