Effect of Mn on the critical strain for completion of DEFT in low carbon steel

TIAN Jing,LIU Jin,YANG Wang-yue,SUN Zu-qing,XUE Wei
DOI: https://doi.org/10.3969/j.issn.1009-6264.2006.04.010
2006-01-01
Abstract:Based on the mechanism of deformation enhanced ferrite transformation (DEFT), the effect of Mn on the critical strain (ε c) for the completion of DEFT were investigated when the undercooled austenite in two different low carbon-manganese steels were deformed at 780°C and strain rate of 10 s -1. The results show that Mn has a strong effect on ε c and the effect on microstructural evolution and transformation kinetics is observed. The transformation process is retarded and ε c increases with increasing Mn content. The microstructure evolution and transformation kinetics can be divided into two stages. The value of curve slope is close to 4 at the first stage, corresponding to the nucleation at primary austenite grain boundaries. The value of curve slope is decreased to 1.0-2.0 at the second stage, corresponding to the nucleation at the areas ahead of formed ferrite grains where new nucleation sites are kept creating till the completion of DEFT. In addition, with increasing Mn ferritic grain size decreases.
What problem does this paper attempt to address?